当前位置:『 产品信息 』


轻烧镁钙粉CALCINED CAUSTIC MAG-LIME POWER

    轻烧镁钙粉是以含钙菱镁石为原料,采用轻烧窑经800℃-1000℃煅烧而成,其特点是含氧钙高,含二氧化硅低,是生产合成镁钙砂,合成镁铁钙砂的理想原料。
    Produced through shaft kil firing at 800℃-1000℃ by using raw magncsite with high Lime content and raw dolomite as raw materials.It has high content of CaO and low content of SiO2.And it is an ideal raw material for the production of synthetic.

产品主要理化指标 Main Physiochemical Property ndexes of product

指标
Index

类别
Category
烧减
LOi
SiO2 Al2O3 Fe2O3 CaO MgO
轻烧镁钙粉
Calcined Caustic Magnesia
A ≤8.00 ≤0.60 ≤0.30 ≈1.00 6-8 ≥85
轻烧镁钙粉
Calcined Caustic Magnesia
B ≤8.00 ≤0.60 ≤0.30 ≈1.00 3-5 ≥82
轻烧镁钙粉
Calcined Caustic Magnesia
C ≤11.00 ≤0.60 ≤0.30 ≈1.00 12-15 ≥72
轻烧镁钙粉
Calcined Caustic Magnesia
D ≤8.00 ≤0.60 ≤0.30 ≈1.00 2-3 ≥87
轻烧白云石
Sintered Dolomite
E ≤12.00 ≤0.40 ≤0.30 0.5-0.7 47-48 36-38
轻烧白云石
Sintered Dolomite
F ≤10.00 ≤0.40 ≤0.30 6-8 44-47 35-37

上一页previous  下一页NEXT